3M 7847 Polyacrylic IUID Labels
Features
- The cast modified polyacrylate facestock has a matte surface that can be marked with a CO2 or YaG laser
- Long-term durability
- Excellent abrasion, temperature, chemical and environmental resistance
- High-resolution, high-contrast label images
- Excellent barcode readability
- Permanent adhesion to LSE plastics, oily metals, powder coatings and textured surfaces
- Description
- Specifications
- Testing Information
- Chemical Testing
- Temperature Testing
- Label Adhesion
Our laser-etched 3M 7847 Polyacrylic IUID Labels provide an excellent alternative for applications that require high-contrast images, reliable readability, long-term durability and flexibility. Extremely resistant to thermal shock and temperature extremes. Polyacrylic UID Labels are virtually impervious to all but the most caustic chemicals. In the same family of plastics as Kevlar® and Lexan®, polyacrylic provides for a long-lasting, very robust asset tag. Polyacrylic material is easy to work with, and simple to train others how to apply it to a variety of surface types.
Material | 3M 7847 Polyacrylic Material |
Serialization | Barcode and human-readable equivalent. Code 39 is the standard symbology with a range of 2.7 to 9.4 CPI (characters per inch). Optional symbologies include Code 128, I 2 of 5, 2D DataMatrix and QR Code |
Label Copy | The label copy my include block type, stylized type, logos or other designs |
Colors | White |
Standard Adhesive | High performance adhesive |
Sizes | Various sizes available |
Packaging | Shipped on sheets |
Shipment | 5 business days |
Chemical Testing Summary
Resistance to chemicals and solvents: samples applied to glass panels, allowed to wet out for 72+ hours, immersed in chemicals below. Ambient room temperature conditions. Key: NE = No Effect, AO = Adhesive Ooze, AL = Loss of Adhesive to Glass Panel, TD = Tag Delaminated, PE = Print Erosion Under Laminate, ER = Adhesive Edge Erosion, TW = Tag Wrinkled
Chemical Testing Data
Immersion Time | Water | Salt Water | Bathroom Cleaner | Glass Cleaner | Alcohol | Brake Fluid | Acetone | Diesel Fuel | Nitric Acid | HCl | NaOH |
---|---|---|---|---|---|---|---|---|---|---|---|
2 hours | NE | NE | NE | NE | AO-ER | NE | TW | AO,ER | NE | NE | NE |
24 hours | NE | NE | NE | NE | TW, AL | TW | TW | AO, ER | NE | NE | NE |
48 hours | NE | NE | NE | NE | TW, AL | TW | TW | AO, ER | NE | NE | NE |
Temperature Testing Summary
Resistance to Extreme Temperatures Key: NE = No Effect
Temperature Testing Data
Temperature | -40 °F (-40 °C) | 450 °F (232.2 °C) |
---|---|---|
Exposure period | 24 hours | 1 hour (max temp exposure) |
Change | NE | NE |
Label Adhesion Summary
Measured according to DIN 306446, Part 1 (300 mm/mm at 180 angle, film with: 25.4 mm. Adhesive performance for each case can depend on the texture of the surface. The above adhesive values are average values. They are not appropriate for specifications.
Label Adhesion Data
Adhesion | Performance/Bond Strength | Performance/Bond Strength |
---|---|---|
Stainless Steel | 108 oz/inch | 30 N/inch |
Aluminum | 108 oz/inch | 30 N/inch |
Polypropylene | 72 oz/inch | 20 N/inch |
Polyethylene | 64 oz/inch | 18 N/inch |
Polycarbonate | 90 oz/inch | 25 N/inch |
ABS | 101 oz/inch | 28 N/inch |
PVC | 108 oz/inch | 90 N/inch |